Austenitic Stainless steel AISI 316; Frequency of 120 Hz; 30 million cycles; Stages I and II of brittle fracture; Stage III of the ductile fracture did not occur. In this test and in the other equivalents Epsilon Martensite was identified by magnetism and quantified. The Epsilon martensite greatly reduces the fatigue strength of AISI 316.